Spraying type chemical copper plating liquid,metal surface rapidly copper plating liquid, Copper plating agent, Large-scale process of copper plating water , Copper protective agent

Product Name:Spraying type chemical copper plating liquid,metal surface rapidly copper plating liquid, Copper plating agent, Large-scale process of copper plating water , Copper protective agent

Price:


Spraying type chemical copper plating liquid,  copper plating liquid,Copper plating process ,metal surface rapidly copper plating liquid, Copper plating agent, Large-scale process of copper plating liquid , Copper protective agent

Spraying type chemical copper plating liquid,metal surface rapidly copper plating liquid, Copper plating agent, Large-scale process of copper plating water , Copper protective agent



First, the product code: Q / YS.121 (Yi Shun brand)


Second, product performance and use:

The products are widely used in large items, stone, stone statues, including plastics, resins, such as large statues, sculpture, crafts, and other large non-metallic and metallic copper surface, simply spraying, not be energized, easy, economical and time-saving Effortless, plated copper layer is copper (pink), can be used for antique copper.


Third, product index:

① product consists of A, B two liquid composition to A: B: water = 1: 2: 3 preparation.

② A agent is blue transparent liquid, B agent is a transparent light yellow liquid.

③ proportion> 1.0

④ PH value> 9


Fourth, the use of methods:

① For metal surfaces, such as iron and nickel surfaces, the plating should be acid activated before spraying copper.

② For non-metallic surfaces, such as large stone, stone, plastic, resin, etc., should be subject to the following:

A. Coarse, polished, finishing, washing, etc., so that the surface is uniform and rough.

B. Activator to dry naturally after activation.

C. Spraying of chemical nickel, so that the surface immediately forms a metallic nickel layer.

D. After washing, immediately spray copper, the workpiece surface quickly plated with a layer of pink copper metal.

③Spray copper preparation: two A and B were heated to 60 ℃, then press A: B: hot water = 1: 2: 3 ratio and immediately mixed into the sprayer, the preparation of a good copper plating water should be 5 All run out in minutes.


Other processingChemical Plating Liquid TrainCopper oil removal passivation agentInferior quality brass environmental chemical polishing agentEnvironment-friendly copper chemical polishing liquid